Fabric Specifications
Yarn | Knitted UV-stabalized HDPE |
Construction | Monofilament & tape |
Pattern | Lock-stitch knitted |
Temperature range (C°) | -30 to +70 |
Approximate thickness (mm) | ~1.6 |
Tensile strength- warp(N/50mm)(AS 2001.2.3.1) | 670 N/50mm |
Elongation at break- weft(%) (AS2001.2.3.2) | 117% |
Wing tear-warp(mean) (AS2001.2.10) | 184N |
Wing tear- weft (mean) (AS2001.2.10) | 347N |
Burst pressure (kPa) (AS4878.5- Method B) | 3500 kPa |
Burst force (N) (AS2001.2.19) | 1937 N |
Flammability Index (range0-100) | 12 |
Lead | Not detected |
Pthalate | Not detected |